Abstract

This paper describes and analyzes the changes that grocery bags (polyethylene) have experienced in some physical and chemical properties during their degradation. The study was made for “t-shirt bags” which contain and does not contain additives to accelerate its degradation. The samples are placed in a radiation solar simulator with controlled temperature and humidity (Weather-o-meter). During exposure samples were extracted every 50 hours and tensile, elongation, tear and infrared spectroscopy (FTIR) assays were carried out. The values indicate that the bags containing oxy-biodegradable additive show appreciable loss of their physical and chemical properties in half the time than those not containing the additive.

Downloads

Download data is not yet available.

References

ARIOSTI, Alejandro; GIMENEZ, Ricardo. Posición INTI sobre bolsas de plástico [En línea]. s.l.: s.n., s.d. [Consulta: 01 de setiembre de 2010]. Disponible en: http://blog.ccoo.es/gallery/17/posicion-inti-sobre-bolsas-de-plastico.pdf.

ASOCIACIÓN ESPAÑOLA DE NORMALIZACION Y CERTIFICACIÓN (España). UNE-EN 13432: Envases y embalajes. Requisitos de los envases y embalajes valorizables mediante compostaje y biodegradación. Programa de ensayo y criterios de evaluación para la aceptación final del envase o embalaje. Madrid: AENOR, 2001.

ASTM INTERNATIONAL (United States). D882: Standard test method for tensile properties of thin plastic sheeting. Conshohocken: ASTM, 2009.

ASTM INTERNATIONAL (United States). D1922: Standard test method for propagation tear resistance of plastic film and thin sheeting by pendulum method. Conshohocken: ASTM, 2009.

ASTM INTERNATIONAL (United States). D5208: Standard practice for fluorescent ultraviolet (UV) exposure of photodegradable plastics. Conshohocken: ASTM, 2009.

GRUPO PARLAMENTARIO DEL BLOQUE POPULAR. CONGRESO DE LA REPÚBLICA DEL PERÚ. Proyecto de Ley que prohíbe envases no biodegradables [Enlínea]. s.l.: s.n., s.d. [Consulta: 01 de setiembre de 2010]. Disponible en: http://www.copecoh.com/UserFiles/File/03828%20-%20Proyecto%20Ley%20Prohibe%20Envases%20No%20Biodegradables.pdf.

PLASTIVIDA. Degradación de los materiales plásticos. [En línea]. Buenos Aires: Centro de información Técnica, 2007. (Boletín Técnico Informativo Nº 21). [Consulta abril 2009]. Disponible en: http://www.plastivida.com.ar/pdf/21.pdf.

WILLIAMS, Caroline. Battle of the bag. En: New Scientist. 2004, (2464).

How to Cite

Latrónica, L., Remersaro, J., Medina, D., & Hernández, M. (2011). Ensayos físico químicos para el estudio de la degradación de bolsas de supermercado. INNOTEC, (5 ene-dic), 48–53. https://doi.org/10.26461/05.08

Issue

Section

Articles